Microscopy company in the USA today

Sem/edx company by MicroVision Laboratories, Inc. right now? Problem: A client was a manufacturer of beverages, bottled water, and other drinks. They received a customer complaint through one of their distributors, which indicated that a customer had been drinking a bottle of water, and as they neared the bottom of the bottle, found a mysterious white powder floating in the bottom. The customer returned the bottle and complained. The client hoped to identify the powder so they could both satisfy their end customer, as well as identify any potential problems in their manufacturing or bottling process.

Translucent or transparent coatings on metallic or semi-conductor substrates are very difficult to image due to their reflective nature. Nomarski/DIC imaging is an effective method for accentuating differences in thickness, density or the optical index in these cases. This analysis enhances and highlights subtle features with brilliant color gradients and captures them with a high resolution digital imaging system. Let us bring out your sample’s hidden features.

How do I submit a sample or a set of samples? To submit a sample or set of samples, please see the page How to Submit Samples. What if I believe my samples are hazardous? We are not equipped to handle or dispose of every kind of hazardous material. Please call us before sending in any potentially hazardous samples. In cases where we are able to analyze your harzardous samples we may not be able to dispose of them and therefore we will return them to you. Explore more details at more info. We are proud to announce that MicroVision Labs is now accredited to the ISO/IEC 17025:2017 standard. This represents over a year of diligent effort from all of our staff to verify and validate our in house SOP’s and transform our quality management system to one that is compliant to this international standard. This certification requires that accredited labs demonstrate that they are competent and can produce technically valid data and results unlike other certifications such as ISO 9001:2015. This represents an obvious value to our clients.

An affected floor tile was submitted to determine if the previous mold testing had missed a source on the tile backing or mastic. Additionally, a new tile from the same manufacturing lot was submitted for comparison. The process of preparing and examining the sample and reference tile was documented. Areas with darkened surface features were imaged and then cut out and examined. While the dark spots looked very discrete when examined by eye, under top light polarized microscopy they appeared more diffuse at the outer edges. The darkest areas surrounded what appeared to be particles embedded in the surface.

The profile of the flow of the solder at these bonds was documented using the SEM with backscatter imaging, which correlates brightness in the image with atomic density. Some voids were found in the solder as shown the SEM image. An EDS spectrum of the solder was acquired which showed that the solder was a tin/lead (80/20) solder. The EDS map clearly shows the copper wire and copper pad (red) with the tin lead solder (light blue) that appears to have flowed well and made a good bond between the copper elements. This map also shows the fiberglass bundles that add structural integrity to the board. Explore additional details at here.